The Analysis of the Effect of Filler Product Types in the Welding Process of STPG 370 Pipe Material in Seawater Pipe Applications Using the Shielded Metal Arc Welding (SMAW) Method with Corrosion Test.
Analisis Pengaruh Jenis Produk Filler dalam Proses Pengelasan Material Pipa STPG 370 pada Aplikasi Pipa Air Laut Menggunakan Metode Shielded Metal Arc Welding (SMAW) dengan Uji Korosi
DOI:
https://doi.org/10.21070/ups.5377Keywords:
Welding, SMAW, Korosi, LB52U, RC52U, E6013Abstract
In the marine industry, there are several cases of damage and leakage in welded seawater pipe joints in marine systems caused by corrosion processes. This comparative research is to find the filler material that is most resistant to corrosion. The filler materials tested were LB52U, RC52U, and E6013. The method used is SMAW welding using AC current and the corrosion test process using the lost weight gain (LWG) method with immersion using Hcl liquid media. The pipe specimen used is STPG370 D125 Sch80. Immersion of the specimen for 8 hours and the obtained corrosion rate value for welding on STPG370 pipe metal with air cooling media and the corrosion rate of LB52U electrode material is 1.026 mm / year, for RC52U electrode material is 0.771 mm / year, for LB52U + E-6013 electrode material is 0.767 mm / year, RC52U + E-6013 electrode material is 0.826 mm / year.
Downloads
References
PT PAL INDONESIA, “Profil Perusahaan-PT PAL Indonesia,” PT PAL INDONESIA web page. [Online]. Available: https://www.pal.co.id/dewan-direksi-3/
C. Pratiwi, “7._BAB_VI_(Piping_System),” pp. 213–285, 2018.
B. W. Ziliwu and M. Tumpu, “Perawatan Sistem Pendingin,” Akselerator J. Sains Terap. dan Teknol., vol. 1, no. 1, pp. 11–19, 2020.
A. Suprayoga and M. Mulyadi, “Experimental Study on AA6005-T6 Material Welded with Friction Stir Welding Using Impact Test,” Indones. J. Innov. Stud., vol. 13, pp. 1–10, 2021, doi: 10.21070/ijins.v13i.532.
ALLPRO, “Pengelasan SMAW.” [Online]. Available: https://www.allpro.co.id/pengelasan/smaw/
H. Wiryosumarto and T. Okumura, “L4H $ fiLT,” Teknol. Pengelasan Logam, vol. 8, 2000.
Aisyah, “Perubahan Struktur Mikro dan Sifat Mekanik pada Pengelasan Drum Baja Karbon Wadah Limbah Radioaktif,” Pus. Teknol. Limbah Radioaktif-BATAN, pp. 159–174, 2011.
T. Natasya, M. E. Khairafah, M. S. Br Sembiring, and L. N. Hutabarat, “Corrosion Factors on Nail,” Indones. J. Chem. Sci. Technol., vol. 5, no. 1, p. 47, 2022, doi: 10.24114/ijcst.v5i1.33159.
M. Ash and I. Ash, Handbook of Corrosion inhibitors, vol. 98, no. 10. 2000. [Online]. Available: https://linkinghub.elsevier.com/retrieve/pii/S0026057600834455
A. Ramaadani, “Analisis Perbedaan Laju Korosi Material Jari-Jari Sepeda Motor (Spokes) Pada Berbagai Media Air yang Berkonsentrasi Asam di Daerah Perindustrian,” Jptm, vol. 06 Nomor 0, pp. 52–57, 2017.
A. Ngatin, Y. Tonapa, R. Regiyanti, and R. Karomi, “Elektroplating Flash Chrome Pada Baja Karbon Rendah,” Pros. Semin. Nas. Kim. UNY 2017, vol. 21, no. 4, pp. 183–188, 2017.
Wanlei, “PIPA STPG370.” Accessed: Oct. 25, 2023. [Online]. Available: http://id.weldsteelpipe.com/steel-pipe/seamless-steel-pipe/stpg370-seamless-steel-pipe.html
Metro Rekayasa, “kawat las kobelco,” metrorekayasa.com. Accessed: Oct. 26, 2023. [Online]. Available: https://metrorekayasa.com/products/welding-consumables/welding-electrode-kobelco-kawat-las-kobelco/
N. Steel, “Manufacturers of a Diverse Range of Hv-600,” 21 Sept. 2023, p. 1, 2014.
P. H. Tjahjanti and H. Bramantyo, “Analysis of corrosion penetration rate (CPR) of exhaust ford laser assembled in 1997 which was coated with chrome (Cr),” AIP Conf. Proc., vol. 1555, no. September, pp. 44–47, 2013, doi: 10.1063/1.4820990.
L. D. Yuono and U. S. Dharma, “Pengaruh Pendinginan Cepat Terhadap Laju Korosi Hasil Pengelasan Baja Aisi 1045,” Turbo J. Progr. Stud. Tek. Mesin, vol. 6, no. 1, pp. 76–83, 2017, doi: 10.24127/trb.v6i1.469.
Downloads
Additional Files
Posted
License
Copyright (c) 2024 UMSIDA Preprints Server
This work is licensed under a Creative Commons Attribution 4.0 International License.